含磷酸钙与磷酸镁的生物活性磷酸盐静电纺PVA纳米纤维
Bioactive phosphate-containing electrospun PVA nanofibers incorporating calcium phosphate and magnesium phosphate
研究将磷酸镁(MgP)与磷酸一钙(MCP)掺入静电纺聚乙烯醇(PVA)纳米纤维,制备出生物矿化潜力增强的骨仿生纳米复合支架。0.5 w/v% 的 MCP 和 MgP 使平均纤维直径从 541 nm 分别降至 284 nm 和 257 nm,分布更窄;最大降解速率温度由纯 PVA 的 280 °C 升至 290 °C 和 300 °C。
- Article
- Open access
- Published: 26 October 2026
- Fatemeh Habibi1,
- Hamed Salimi-Kenari ORCID: orcid.org/0000-0003-3305-57051,
- Seyed Reza Nabavi2 &
- …
- Parisa Nikpour1
Scientific Reports (2026) Cite this article
We’re sharing this article early to provide faster access to peer-reviewed, accepted research. It is citable and carries a permanent DOI. This version is subject to further edits and will be replaced automatically by the final Version of Record. All legal disclaimers apply.
Abstract
Bone-mimetic scaffolds are pivotal components in bone tissue engineering, particularly those exhibiting intrinsic bioactive characteristics. This study presents nanocomposite scaffolds with enhanced biomineralization potential based on electrospun poly(vinyl alcohol) (PVA) nanofibrous matrices incorporating magnesium phosphate (MgP) and monocalcium phosphate (MCP). FTIR analysis revealed the formation of non-covalent interactions, such as hydrogen bonds and electrostatic attractions, between the nanoparticles and the PVA chains, confirming their successful incorporation. The incorporation of 0.5 w/v% MCP and MgP contributed to a reduction in the average fiber diameter from 541 nm for the PVA/surfactant formulation to 284 and 257 nm, respectively, while producing narrower fiber diameter distributions. Increasing MCP or MgP concentrations from 0.5 to 1.5 w/v% led to a non-linear variation in fiber diameter, with the average fiber diameter initially increasing and then decreasing. Strong intermolecular interactions between PVA and phosphate phase enhanced thermal stability of the composite scaffolds, as evidenced by the increase in the temperature of the maximum degradation rate from 280 °C for neat PVA to 290 °C and 300 °C for PVA/MCP and PVA/MgP, respectively. After 21 days of immersion in simulated body fluid (SBF) at 37 °C, SEM, EDX, and XRD analyses confirmed the substantial surface mineralization and phase transformation in both composite systems. The PVA/MCP scaffolds predominantly developed hydroxy apatite-like calcium phosphate, whereas PVA/MgP scaffolds exhibited newberyite and bobierrite phases. The results reveal that incorporation of MCP and MgP modulates the physicochemical properties and biomineralization behavior of electrospun PVA nanofibers.
Funding
This research did not receive any specific grant from funding agencies in the public, commercial, or not-for-profit sectors.
Author information
Authors and Affiliations
Department of Chemical Engineering, Faculty of Engineering, University of Mazandaran, Babolsar, Iran
Fatemeh Habibi, Hamed Salimi-Kenari & Parisa Nikpour
Department of Applied Chemistry, Faculty of Chemistry, University of Mazandaran, Babolsar, Iran
Seyed Reza Nabavi
Authors
- Fatemeh Habibi
- Hamed Salimi-Kenari
- Seyed Reza Nabavi
- Parisa Nikpour
Corresponding author
Correspondence to Hamed Salimi-Kenari.
Ethics declarations
Competing interests
The authors declare no competing interests.
Additional information
Publisher's note
Springer Nature remains neutral with regard to jurisdictional claims in published maps and institutional affiliations.
Rights and permissions
Open Access This article is licensed under a Creative Commons Attribution 4.0 International License, which permits use, sharing, adaptation, distribution and reproduction in any medium or format, as long as you give appropriate credit to the original author(s) and the source, provide a link to the Creative Commons licence, and indicate if changes were made. The images or other third party material in this article are included in the article’s Creative Commons licence, unless indicated otherwise in a credit line to the material. If material is not included in the article’s Creative Commons licence and your intended use is not permitted by statutory regulation or exceeds the permitted use, you will need to obtain permission directly from the copyright holder. To view a copy of this licence, visit http://creativecommons.org/licenses/by/4.0/.
About this article
Cite this article
Habibi, F., Salimi-Kenari, H., Nabavi, S.R. et al. Bioactive phosphate-containing electrospun PVA nanofibers incorporating calcium phosphate and magnesium phosphate. Sci Rep (2026). https://doi.org/10.1038/s41598-026-77740-x
Received: 06 July 2026
Accepted: 21 October 2026
Published: 26 October 2026
DOI: https://doi.org/10.1038/s41598-026-77740-x
Keywords
来源:Nature Biotechnology · nature.com